2021-01-30
	
	 
		42.5復(fù)合硅酸鹽水泥
	 
		42.5 Composite Portland Cement
	
	
| 
					 項(xiàng)目 Project  | 
				
					 國家標(biāo)準(zhǔn) GB175—2007  | 
				
					 本廠實(shí)際 Actual level  | 
			||
| 
					 抗折強(qiáng)度(MPa) Break strength  | 
				
					 3天(3Days)  | 
				
					 ≥3.5  | 
				
					 ≥4.5  | 
			|
| 
					 28天(28Days)  | 
				
					 ≥6.5  | 
				
					 ≥8.0  | 
			||
| 
					 抗壓強(qiáng)度(MPa) Compression strength  | 
				
					 3天(3Days)  | 
				
					 ≥15.0  | 
				
					 ≥20.0  | 
			|
| 
					 28天(28Days)  | 
				
					 ≥42.5  | 
				
					 ≥46.5  | 
			||
| 
					 
						凝結(jié)時(shí)間(min)  | 
				
					 初凝時(shí)間 Coagulating start time  | 
				
					 ≥45  | 
				
					 100—300  | 
			|
| 
					 終凝時(shí)間 Coagulating end time  | 
				
					 ≤600  | 
				
					 200—400  | 
			||
| 
					 細(xì)度 (45μm篩)(%)  | 
				
					 ≤30.0  | 
				
					 ≤20  | 
			||
| 
					 SO3 (%)  | 
				
					 ≤3.5  | 
				
					 ≤3.0  | 
			||
| 
					 MgO (%)  | 
				
					 ≤6.0  | 
				
					 ≤5.0  | 
			||
| 
					 氯離子(%) Chloride ion  | 
				
					 ≤0.06  | 
				
					 ≤0.05  | 
			||
| 
					 安定性(沸煮法)  | 
				
					 合格  | 
				
					 合格  | 
			||
| 
					 備 注  | 
				
					 若用戶要求提供低堿水泥時(shí),則水泥中堿含量小于0.6%。  | 
			|||
| 
					 特點(diǎn)  | 
				
					 強(qiáng)度高,凝結(jié)時(shí)間適中,水泥流動(dòng)性好。  | 
			|||
| 
					 適用范圍  | 
				
					 海港、鐵路、橋梁等混凝土工程。  | 
			|||